Mastars

Location: Home » Resources » FAQ
Related news
FAQ and solutions for metal cutting processes
FAQ and solutions for metal cutting processes
Mastars is a metal prototype maker, Mastars uses CNC technology to make prototypings and functional parts, providing cus...
Understand the sheet metal processing process|metal prototype maker
Understand the sheet metal processing process|metal prototype maker
Mastars is ametal prototype maker, engaged in sheet metal processing, precision sheet metal processing, Chinese sheet me...
What are the characteristics of ABS materials used for handboard production?
What are the characteristics of ABS materials used for handboard production?
Mastars is a company specializing in prototyping, rapid prototyping, CNC parts processing, 3D printing, laser forming, s...
3D Printing Prototyping: definition, process, advantages, applications
3D Printing Prototyping: definition, process, advantages, applications
Here's a detailed explanation of 3D Printing Prototyping, covering its definition, process, advantages, applications.Rap...
Rapid Prototyping Tooling Definition, methods,technologies
Rapid Prototyping Tooling Definition, methods,technologies
Rapid Tooling (RT) is a broad term for a set of techniques that use additive manufacturing (3D printing) or other rapid...
Tighter Tolerance Requirements Promote Micro Molding Technology Innovation
Tighter Tolerance Requirements Promote Micro Molding Technology Innovation
|CNC machining company |CNC machining services|Customized 3D Printing Service ?Materials research is still one of the m...
Surface treatment process(1)|rapid cnc machining|Mastars
Surface treatment process(1)|rapid cnc machining|Mastars
The purpose of surface treatment is to meet the requirements of corrosion resistance, wear resistance, decoration or oth...
What is the most difficult material for sheet metal bending
What is the most difficult material for sheet metal bending
Mastars often uses the sheet metal process to make prototypes and carry out mass production. The sheet metal process is ...
Glossary of Plastic Injection Molding Terms
Glossary of Plastic Injection Molding Terms
An A to Z guide to terminologies in Injection tooling.Here is a detailed English-language guide to the professional term...

Contact us

  • Building 6 , Blue Sky Industrial Park, Ditang Road, Shajing Town, Shenzhen City,Guangdong, China (518104)
  • marketing@mastars.com

Polypropylene (PP) injection molding process|Mastars

Release date:01 , Jan , 0001 Source:Mastars Pageviews:-
PP is generally known as polypropylene, also known as "100% gel" because of its good breaking resistance. PP is a translucent, semi crystalline thermoplastic, which has the characteristics of high strength, good insulation, low water absorption, high thermal deformation temperature, low density and high crystallinity. Modified fillers usually include glass fiber, mineral filler, thermoplastic rubber, etc.

Contents

Mastars

3D printing 

injection molding

rapid prototype

生产车间02(1)


PP is generally known as polypropylene, also known as "100% gel" because of its good breaking resistance. PP is a translucent, semi crystalline thermoplastic, which has the characteristics of high strength, good insulation, low water absorption, high thermal deformation temperature, low density and high crystallinity. Modified fillers usually include glass fiber, mineral filler, thermoplastic rubber, etc.


The fluidity of PP for different purposes varies greatly. Generally, the flow rate of PP is between ABS and PC.

Pure PP is translucent ivory white, which can be dyed into various colors. PP dyeing can only use color masterbatch on general injection molding machines. In some machines, there are independent plasticizing elements that strengthen the mixing effect, and they can also be dyed with toner. Products used outdoors are generally filled with UV stabilizer and carbon black. The use proportion of recycled materials should not exceed 15%, otherwise it will cause strength reduction and decomposition discoloration. PP generally does not need special drying treatment before injection molding.


There are no special requirements for the selection of injection molding machines. Because PP has high crystallinity. Computer injection molding machine with high injection pressure and multi-stage control is required. The clamping force is generally determined by 3800t/m2, and the injection amount is 20% - 85%.


The mold temperature is 50-90 ℃, and high mold temperature is used for those with high dimensional requirements. The core temperature is more than 5 ℃ lower than the cavity temperature, the runner diameter is 4-7mm, the needle gate length is 1-1.5mm, and the diameter can be as small as 0.7mm. The shorter the length of the side gate, the better, about 0.7mm, the depth is half of the wall thickness, and the width is twice the wall thickness, and increases with the length of the melt flow in the mold cavity. The mold must have good exhaust performance. The exhaust hole is 0.025mm-0.038mm deep and 1.5mm thick. To avoid shrinkage marks, large and round injection ports and circular flow channels should be used, and the thickness of stiffeners should be small (for example, 50-60% of the wall thickness). The thickness of products made of homopolymer PP should not exceed 3mm, otherwise there will be bubbles (thick wall products can only use copolymer PP).


The melting point of PP is 160-175 ℃, the decomposition temperature is 350 ℃, but the temperature setting during injection processing cannot exceed 275 ℃, and the melting section temperature is preferably 240 ℃.

In order to reduce internal stress and deformation, high-speed injection should be selected, but some grades of PP and mold are not applicable (bubbles and wrinkles appear). If there are bright and dark stripes diffused by the gate on the engraved surface, low-speed injection and high mold temperature should be used.


5bar melt back pressure can be used, and the back pressure of toner can be adjusted appropriately.


Adopt higher injection pressure (1500-1800bar) and holding pressure (about 80% of the injection pressure). Turn to pressure maintaining at about 95% of the full stroke, and use a longer pressure maintaining time.

In order to prevent shrinkage deformation caused by post crystallization, products generally need to be soaked in hot water.